hello
this is a calling for the gurus of lamination, looking for help. i have some problems ; firstly it appears fish eye and the fiber doesn´t fix well with epoxy.
I use a fiber glass 83grm and carbon, the working temperature is 27+- .
I´m waiting for your help.
regards.



View User's Profile Visit User's Homepage View All Posts By User U2U Member
Whitemouse





Posts: 90
Registered: 27-4-2007
Location: Copenhagen, Denmark
Member Is Offline
Mood: Life is GREAT!!!
posted on 3-8-2010 at 13:10 Reply With Quote


Funmaker, first of all I think you have to work a little harder at the gel-coat! You have to keep on brushing until the gel-coat/bottom coat lays evenly spread over the whole surface of the mold.

83 grams/m2 seems a bit rough/heavy for my taste, I use 40 grams/m2 glassfiber mats myself.

The Epoxy is from Dutch Poly Service www.polyservice.nl

Good luck




Cheers,
Paal Hanson
Vikings Scaleracing Club, Frederikssund, Denmark
View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
fumaker





Posts: 9
Registered: 15-6-2006
Member Is Offline
Mood: No Mood
posted on 8-8-2010 at 21:58 Reply With Quote


thanks a lot for your comments; just one more question: how many coats of epoxy do you aply and how many fiber glass coats do you put one over another? thank you for the help, if you had any other suggestions I would be very thankfull.
View User's Profile Visit User's Homepage View All Posts By User U2U Member
Whitemouse





Posts: 90
Registered: 27-4-2007
Location: Copenhagen, Denmark
Member Is Offline
Mood: Life is GREAT!!!
posted on 13-8-2010 at 19:23 Reply With Quote


One bottom layer or gel-coat, as thin as posible. Normaly I have cut out different size fibre glass pieces ranging from stamp size to say 20 x 100 mm and when laminating I try to get the pieces to overlap each other so I only get one complete layer of fiber glass mats.

I do put some extra material in the front and rear.

I think Tamar has an old article about all of this somewhere on this site!?! Tamar, link please!




Cheers,
Paal Hanson
Vikings Scaleracing Club, Frederikssund, Denmark
View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
gabe2001
LMSadmin




Posts: 157
Registered: 23-6-2002
Member Is Offline
Mood: U = R * I
posted on 14-8-2010 at 17:30 Reply With Quote


link to hotslot workshop article: http://www.slotracinglemans.com/newforum/news.php?action=view&catid=3&aid=136

my photonovela about laminating an acura lmp2 body: http://picasaweb.google.com/gabe.inabnit/LaminatingA124ScaleAcuraBody

a hint I got from Fola: wait 15-20 minutes before applying the "gel coat" after mixing the two components - no need to try to apply the not so sticky mixture, just wait until it's stickier. Another help are cotton fibres. Mix them with your gel coat mixture for faster sticking to silicone mould (haven't tried that personally yet)
View User's Profile Visit User's Homepage View All Posts By User U2U Member
CanAm





Posts: 1
Registered: 12-12-2011
Location: Poppel Belgium
Member Is Offline
Mood: No Mood
posted on 12-12-2011 at 18:10 Reply With Quote


Hello everybody,

I'm new here and I have some questions about this theme!!

I'm planning to make some GFK body's of the body's I'm modifying at this moment.

I allready have bought the gelcoat (white) and a Peroxide (witch a must mix between 0.25 and 2%) and the glasvlies (in Dutch) 25gr/m2.
Is it necesarry to mix some parafine true this? I heard otherwise the body stays sticky. Is that correct?
How much of the Peroxide must I mix with it? Closer to 0,25% ore 2%?

Thanks in advance.
Maurits
View User's Profile View All Posts By User U2U Member
tamar





Posts: 804
Registered: 5-1-1989
Location: Gouda
Member Is Offline
Mood: A new beginning ;)
posted on 10-1-2013 at 12:43 Reply With Quote


Hello Maurits

Sorry for the late reply, did not notice your post till now.

Not really sure what you are referring to.

Usually all the guys here use the same resin to laminate and do the Gel coat.
No need for Parrafine nor Peroxide so I'm affraid we cant help you with this question.




With kind regards
Tamar
View User's Profile E-Mail User Visit User's Homepage View All Posts By User U2U Member
fumaker





Posts: 9
Registered: 15-6-2006
Member Is Offline
Mood: No Mood
posted on 26-1-2013 at 14:20 Reply With Quote


hi tamar!
i would like to ask you how many grams of resin do you use on the first gel coat to prevent the fish eyes?